Processo térmico

Nitriding Powder and Activator, Boriding Powder
  
  
PRODUCT IMAGE

Nitriding powder

  • Workpieces are placed into an annealing box together with the nitriding powder and activator and the lid is closed and sealed
  • Powder nitriding or powder boriding causes a thin cover layer to form against friction wear and fatigue resistance is substantially increased
  • At approx. 550 °C an extremely thick cover layer forms (up to 1000 HV) which covers the hardened steel or the carburized edge layer. The activator improves process conditions.
  • The process duration at 550 °C is at least 10 hrs
  • For all steels and cast iron, such as hot work steel matrices, injection molding dies, wear parts and machine components
  • Anti-nitriding paste to protect areas which should not be processed
  • Boriding powder upon request
Article no.DescriptionContainer
491010250Nitriding powder80 kg
491010150Activator25 kg
491010100Activator 5 kg
491003000Anti-nitriding paste 1 kg