Nitriding powder |
- Workpieces are placed into an annealing box together with the nitriding powder and activator and the lid is closed and sealed
- Powder nitriding causes a thin cover layer to form against friction wear and fatigue resistance is substantially increased
- At approx. 550 °C an extremely thick cover layer forms (up to 1000 HV) which covers the hardened steel or the carburized edge layer. The activator improves process conditions.
- The process duration at 550 °C is at least 10 hrs
- For all steels and cast iron, such as hot work steel matrices, injection molding dies, wear parts and machine components
- Anti-nitriding paste to protect areas which should not be processed
Article no. | Description | Container |
491010250 | Nitriding powder | 100 kg |
491010150 | Activator | 35 kg |
491010100 | Activator | 5 kg |
491003000 | Anti-nitriding paste | 2 kg |
Thermal Process Technology I (URL: http://www.nabertherm.de/produkte/thermprozesstechnik/thermprozesstechnik_englisch.pdf)